Low Pressure Casting

Low pressure casting fills the mould from below, slowly and without turbulence — the reason it produces the soundest aluminium castings of the three aluminium routes.

Process Introduction

Low Pressure Casting Overview

In low pressure casting, compressed air pushes metal up a riser tube into the mould from a sealed holding furnace. Filling is smooth and the part solidifies while still connected to a reservoir of liquid metal, so shrinkage is continuously fed and gas entrapment is minimal.

That combination is why the process is used for wheels, pressure-tight housings and structural parts where density matters more than cycle time. It is slower than die casting and needs a purpose-built machine and tooling, so it earns its place on parts where porosity would otherwise cause leaks, rejections or fatigue failures.

Quick Facts

  • Typical weight 1 – 25 kg
  • Bottom filling, low turbulence, low gas entrapment
  • Continuous feeding during solidification
  • Good for pressure-tight and fatigue-loaded aluminium parts
  • Slower cycle than die casting, better soundness
Production Flow

How Low Pressure Casting Works

1

Part & Tool Design

2

Permanent Mould Making

3

Furnace & Riser Setup

4

Low Pressure Filling

5

Solidification Under Pressure

6

Demoulding

7

Heat Treatment

8

Machining

9

Leak & X-ray Inspection

+

Advantages

  • Lowest porosity of the aluminium casting routes
  • Excellent feeding on thick and isolated sections
  • Good mechanical properties after T6 treatment
  • Reliable leak-tightness on sealed parts
-

Limitations

  • Slower cycle and higher unit cost than die casting
  • Tooling and machine investment needed
  • Geometry constrained by permanent mould ejection
  • Not economic at very low volume

Suitable Materials

A356 / A356-T6AlSi7MgAlSi10MgAlSi11 (wheel alloys)

Grades are confirmed at drawing review; composition and mechanical properties are verified before shipment.

Suitable Products

Wheels and wheel hubsPressure-tight pump and compressor housingsMotor and inverter housingsStructural covers and bracketsValve bodies for sealed duty

Typical part types for this process. Variants of these are quoted as variants rather than new developments.

Equipment & Technical Parameters

Typical Low Pressure Casting Capability

Each figure is confirmed for your part at drawing review, and the agreed values are written into the quotation.

ParameterTypical capabilityStatus
Casting weight1 – 25 kgpart dependent
Maximum envelopeapprox. 600 × 600 × 400 mmmachine dependent
Minimum wall thickness3 – 4 mmgeometry dependent
Dimensional toleranceISO 8062 CT5 – CT8critical features agreed per drawing
Porositylow; verified by X-ray on critical sectionsper drawing callout
Heat treatmentT6 typical for structural partsper drawing callout
Production volumethousands to tens of thousands per yearper part number
Quality Inspection

How Low Pressure Casting Parts Are Verified

Inspection scope is agreed at order; the quotation lists the checks included.

X-ray

Radiographic check of critical sections, first article and sampled in production.

Leak

Air or water leak test on sealed housings, with recorded pressure and hold time.

Mechanical

Tensile, elongation and hardness after heat treatment.

Dimensional

CMM check of bores, faces and mounting features.

Representative Project Profiles

Typical Projects

Anonymised descriptions of typical projects. Weights, materials and operations are representative of work we run; customer names and drawings are omitted by agreement.

Representative Project 01 — Pressure-tight pump housing

Low pressure · A356-T6

Housing around 9 kg, T6 treated, machined faces and bores, leak tested at 0.3 MPa with no rejects in the first batch.

Representative Project 02 — Motor housing

Low pressure · AlSi10Mg

Housing around 6 kg with cooling ribs, machined stator seat and end-plate faces, X-ray checked on the ribbed wall.

Representative Project 03 — Structural cover

Low pressure · A356-T6

Cover around 4 kg with thick bolted bosses, T6 treated, machined and dimensionally reported against a 40-characteristic drawing.

FAQ

Low Pressure Casting Questions

When the part must be leak-tight or fatigue-loaded, and porosity from high-speed injection would cause rejects in service. If the part is a simple thin cover at high volume, die casting remains cheaper and we will say so.
Yes. Wheel-type parts with a hub and spokes are a classic low pressure application, and the process suits the section transitions where a die casting would leave shrinkage porosity.
No. It is specified when the drawing calls for higher strength or elongation, and it has to be matched to wall thickness to avoid distortion. Untreated parts are supplied as-cast with the condition stated.
Tooling normally takes four to seven weeks from drawing approval, then trial castings, heat treatment and first-article inspection follow before serial production.
Related Pages

Process and Product Pages

Die Casting

View page

Gravity Casting

View page

Housings and Enclosures

View page

Compare all seven casting processes

Have a low pressure casting project?

Send your drawing and requirements; we will confirm process fit, machining scope and price.