Centrifugal Casting

Centrifugal casting uses rotation instead of risers to feed a part: metal is thrown against the mould wall, impurities collect on the bore, and the result is a dense, fine-grained cylindrical section.

Process Introduction

Centrifugal Casting Overview

In true centrifugal casting the mould spins while metal is poured, so centrifugal force holds the metal against the wall until it solidifies. Feeding happens through the whole section rather than through a riser, which is why the structure is dense and why shrinkage porosity is rare in the cast wall.

The process is essentially for rotationally symmetric parts: tubes, sleeves, bearing bushes, roll shells, cylinder liners and rings. Near-net-shape cylindrical parts can be produced with very little machining — usually the bore, the outside diameter and the end faces, with the bore machined to remove the impurity layer that collects there.

Quick Facts

  • Typical weight 5 – 800 kg
  • Rotationally symmetric parts: tubes, sleeves, rings
  • Dense structure, low shrinkage porosity
  • Bore machined to remove the inner impurity layer
  • Iron, steel, stainless, copper and nickel alloys
Production Flow

How Centrifugal Casting Works

1

Mould Preparation & Coating

2

Mould Rotation

3

Pouring

4

Solidification Under Rotation

5

Demoulding

6

Cutting to Length

7

Heat Treatment

8

Bore & Face Machining

9

Inspection

+

Advantages

  • Dense, fine-grained structure without risers
  • High material yield on cylindrical parts
  • Good dimensional consistency along the length
  • Impurities concentrated at the bore, easily machined away
-

Limitations

  • Rotationally symmetric geometry only
  • Bore quality needs a machining allowance
  • Not suitable for complex external features
  • Length and diameter limited by the machine

Suitable Materials

Grey and ductile ironCarbon and low-alloy steelStainless steelCopper alloys (bronze, brass)Nickel-based alloys on review

Grades are confirmed at drawing review; composition and mechanical properties are verified before shipment.

Suitable Products

Cylinder linersBearing bushes and sleevesRoll shells and mill rollsPipe and tube sectionsWear rings and seal rings

Typical part types for this process. Variants of these are quoted as variants rather than new developments.

Equipment & Technical Parameters

Typical Centrifugal Casting Capability

Each figure is confirmed for your part at drawing review, and the agreed values are written into the quotation.

ParameterTypical capabilityStatus
Casting weight5 – 800 kgmachine and part dependent
Outside diameterapprox. 80 – 800 mmmachine dependent
Wall thickness8 – 80 mmprocess dependent
Lengthup to approx. 3,000 mmmachine dependent
Dimensional toleranceISO 8062 CT9 – CT11 as cast, plus machiningcritical features agreed per drawing
Machiningbore, outside diameter and end facesper drawing callout
Production volumesingle pieces to serial runsper part number
Quality Inspection

How Centrifugal Casting Parts Are Verified

Inspection scope is agreed at order; the quotation lists the checks included.

Ultrasonic

UT on the wall for internal soundness where specified.

Dimensional

Bore, outside diameter, wall thickness and straightness checks.

Chemistry

Spectrometric analysis per heat, with hardness on machined faces.

Surface

Visual and penetrant inspection of machined bores.

Representative Project Profiles

Typical Projects

Anonymised descriptions of typical projects. Weights, materials and operations are representative of work we run; customer names and drawings are omitted by agreement.

Representative Project 01 — Cylinder liner

Centrifugal · grey iron

Liner 210 mm bore, 480 mm length, around 22 kg, bore machined and honed to the drawing clearance.

Representative Project 02 — Bronze bearing sleeve

Centrifugal · bronze

Sleeve 180 mm OD, around 14 kg, bore and outside diameter machined, oil grooves cut after machining.

Representative Project 03 — Mill roll shell

Centrifugal · alloy iron

Shell around 620 kg with a hard outer layer, machined bore and journals, UT checked on the wall.

FAQ

Centrifugal Casting Questions

Impurities and any looseness collect on the inner surface during rotation, so a machining allowance is left there and cut away. The finished bore is then the clean, dense material, which is why bore machining is standard rather than optional.
No. The process is for rotationally symmetric geometry. If the part has flanges, ports or asymmetric features, we usually combine a centrifugal tube with a machined or welded flange, or recommend a different process.
Up to roughly 3,000 mm on the current equipment, with length-to-diameter ratio confirmed against the drawing because very slender parts can deflect during rotation.
Iron, steel, stainless and copper alloys are all routine. Nickel-based and other high-alloy grades are quoted on review, since they need different mould coatings and pouring practice.
Related Pages

Process and Product Pages

Sand Casting

View page

Impeller Castings

View page

Mining Machinery Parts

View page

Compare all seven casting processes

Have a centrifugal casting project?

Send your drawing and requirements; we will confirm process fit, machining scope and price.

Request a Quote