Investment Casting (Lost Wax)

When the drawing has thin walls, fine detail and features that should not be machined from a rough casting, investment casting is usually the cheaper route once machining is counted in.

Process Introduction

Investment Casting Overview

Investment casting builds a ceramic shell around a wax pattern, so the mould has no parting line in the usual sense and no sand to compact around complex geometry. That is why it holds thin sections and sharp detail better than sand casting, and why the as-cast surface arrives close enough to the finished shape that machining is limited to functional faces.

The trade-off is pattern cost and size. A wax injection tool is needed before the first part, which makes investment casting best suited to parts that repeat, or to geometries where sand casting would need expensive core work and heavy machining. We use it most for valve bodies, impellers, pump trim, food and chemical industry parts and small structural components in stainless and duplex.

Quick Facts

  • Typical casting weight 0.05 – 80 kg
  • Wall thickness down to 1.5 mm on small parts
  • Tolerance ISO 8062 CT5 – CT7
  • Stainless, duplex, carbon and alloy steel, brass
  • Wax tooling required before first part
Production Flow

How Investment Casting Works

1

Wax Pattern Injection

2

Pattern Assembly

3

Shell Building

4

Dewaxing & Sintering

5

Melting & Pouring

6

Shell Removal

7

Cutting & Grinding

8

Heat Treatment

9

Machining & Inspection

+

Advantages

  • Thin walls and fine detail held without heavy machining
  • No draft-angle compromise on complex geometry
  • Good as-cast surface, less finishing stock
  • Alloy flexibility including stainless and duplex
-

Limitations

  • Wax tooling cost before the first part
  • Practical size limit well below sand casting
  • Higher unit price at very low volume
  • Thick sections cool slower than in sand moulds

Suitable Materials

Carbon steelStainless CF8 / CF8MDuplex 4A / 5AAlloy steelBrass / bronze

Grades are confirmed at drawing review; composition and mechanical properties are verified before shipment.

Suitable Products

Valve bodies and bonnetsPump impellersPump trim and wear ringsFood and chemical fittingsSmall structural parts

Typical part types for this process. Variants of these are quoted as variants rather than new developments.

Equipment & Technical Parameters

Typical Investment Casting Capability

Each figure is confirmed for your part at drawing review, and the agreed values are written into the quotation.

ParameterTypical capabilityStatus
Casting weight0.05 – 80 kgpart and geometry dependent
Maximum envelopeapprox. 600 × 500 × 400 mmtree layout dependent
Minimum wall thickness1.5 – 2.5 mmsmall parts at the lower end
Dimensional toleranceISO 8062 CT5 – CT7critical features agreed per drawing
As-cast surfaceRa 6.3 – 12.5 µm typicalper drawing callout
Production volumefrom a few hundred pieces per yearwax tooling amortised over the run
Material gradescarbon, stainless, duplex, alloy steel, brassequivalent grades confirmed at review
Quality Inspection

How Investment Casting Parts Are Verified

Inspection scope is agreed at order; the quotation lists the checks included.

Chemistry

Spectrometric analysis of each heat before pouring.

Radiography

X-ray of critical sections where specified.

Penetrant

Dye penetrant on machined and cast surfaces.

Dimensional

CMM check of toleranced features and wall sections.

Representative Project Profiles

Typical Projects

Anonymised descriptions of typical projects. Weights, materials and operations are representative of work we run; customer names and drawings are omitted by agreement.

Representative Project 01 — Stainless valve body

Investment · CF8M

Body around 6 kg with cored passage and seat detail, machined only on seat faces and flanges, shell tested before assembly.

Representative Project 02 — Closed impeller

Investment · CF8M

Impeller around 3 kg with 2.5 mm blades, wax tooling built from the 3D model, hub and bore machined to running clearance.

Representative Project 03 — Duplex pump trim

Investment · duplex 4A

Wear ring and throat bush set around 1.5 kg each, cast to near-net shape with only bore and face machining.

FAQ

Investment Casting Questions

When the part is small or medium, repeats over a run, and the sand route would need expensive cores plus heavy machining. If your part is large and simple, sand casting stays cheaper even after machining, and we will say so in the quotation.
Yes, but thick sections cool more slowly in a ceramic shell than in sand, so feeding and shell preheat have to be planned for them. Above roughly 80 kg the sand route is normally the better choice.
Typically two to three weeks after drawing approval, depending on the number of pattern cavities. The tool belongs to the project and stays available for repeat orders.
Yes. Machining scope is agreed at quotation: often only seat faces, bores and flange faces on investment castings, because the as-cast geometry is already close to final.
Related Pages

Process and Product Pages

Sand Casting

View page

Valve Castings

View page

Impeller Castings

View page

Compare all seven casting processes

Have a investment casting project?

Send your drawing and requirements; we will confirm process fit, machining scope and price.

Request a Quote